• başlyk_banner_01

ExxonMobil 1018 mLLDPE plýonkasy

Gysgaça düşündiriş:

ExxonMobil brendi

mLLDPE| MI=1.0

Birleşen Ştatlarda öndürilen


  • Bahasy:1000-1200 ABŞ dollary/MT
  • Port:Huangpu / Ningbo / Şanhaý / ingingdao
  • MOQ:1*40GP
  • CAS belgisi:25213-02-9
  • HS kody:3901402090
  • Töleg:TT/ LC
  • Önümiň jikme-jiklikleri

    Beýany

    Exceed™ 1018 etilen 1-geksen kopolimer smolalarydyr. Exceed™ 1018 smolalaryndan ýasalan filler ajaýyp dartgynlyk täsirine we deşilme güýjüne eýedir. Bu ýokary berklik häsiýetleri, ajaýyp çekiş ukyby bilen birlikde, halta goşundylarynda ölçegleri peseltmäge mümkinçilik berýär. InPP Exceed™ 1018 rezinalaryna bilgeşleýin goşulmaýar.

    Umumy

    Elýeterlilik  · Afrika we Ýakyn Gündogar · Ýewropa · Demirgazyk Amerika
    · Aziýa Ýuwaş ummany · Latyn Amerikasy  
    Goşundy     ·Exceed™ 1018MK: Antiblok: 5000 ppm;Syrgaýyş: 1000 ppm; Işläp düzüji kömekçi: Hawa; Termostabilizator: Hawa
    ·Exceed™ 1018MF:Garyşga blok 4500 ppm; Taýgalyk:450 ppm;Işleýiş usuly:Hawa Termal Durnuklaşdyryjy: Hawa
    ·Exceed™ 1018MA:Bloklama garşy:Ýok; Taýga:Ýok; Işläp bejeriş kömegi:Hawa; Termal stabilizator.Hawa
    ·Exceed™ 1018M): Antiblok: 4500 ppm; Taýga: Ýok; Işläp bejeriş kömegi: Hawa; Termal stabilizator: Hawa
    ·Exceed™ 1018MB:Garyşga blok:2500 ppm; Syrgy:800 ppm; Işläp düzüji kömekçi:Hawa;Termostabilizator:Hawa
    Programmalar       · Oba hojalyk filmi
    · Fom Fil we Möhür Gaplama · OverwrapFilm
    · Gutydaky sumka · Doňduryjy plýonka · Gaplama plýonkalary
    · Azyk üçin päsgelçilikli gaplama · Umumy gaplama · Premium zibil haltalary
    · Üflenen film · Agyr ýük üçin sumkalar · Dik duran haltalar
    · Üflenen streç plýonkasy · Senagat gaplamasy · Zibil haltalary
    · Çörek haltalary · Laminasiýa üçin film · Zibil gutularynyň astarlary
    · Azyk gaplamasy · Köp gatlakly gaplama plýonkasy  
    Gaýtadan gözden geçiriliş senesi · 07/12/2022
    Rezin häsiýetleri Adaty gymmatlyk (iňlis dilinde) Tipiki Baha (SO) Synag esasynda
    Dykyzlyk / Aýratyn agyrlyk 0.918 g/sm³ 0.918 g/sm³ ASTM D792
    Eriş indeksi (190°C/2.16kg) 10 g/10 min 1.0 g/10 min ASTM D1238
    Iň ýokary ereme temperaturasy 244 °F 118 ℃ ExxonMobl usuly
    Filmiň aýratynlyklary Adaty gymmatlyk (iňlis dili) Tipiki Baha (S0 Synag esasynda
    Dartgynlylyk güýji, MD 1300 psi 8.7 MPa ASTM D882
    Çykaryş wagtyndaky dartgynlylyk güýji TD 1300 psi 88 MPa ASTM D882
    Dartgynlylyk güýji MD 9400 psi 60 MPa ASTM D882
    TD-de dartgynlylyk güýji 8400 psi 60 MPa ASTM D882
    Break MD-de Bongation 500% 500% ASTM D882
    Break TD-de Bongasiýa 640% 640% ASTM D882
    Sekant Moduly MD- 1% Sekant 24000 psi 170 MPa ASTM D882
    Sekant Moduly TD-1% Sekant 26000 psi 180 MPa ASTM D882
    Dart DropImpact 550 g 550 g ASTM D1709A
    Emendorf gözýaşynyň güýjiMD 2209 220 g ASTM D1922
    Emendorf gözýaş güýji TD 370 g 3709 ASTM D1922
    Öňünden deşmek 13 funt 59 D ExxonMobil usuly
    Deşik energiýasy 49 dýuým-lb 5.5J ExxonMobil usuly

     

    Optiki häsiýetler Adaty gymmatlyk (iňlis dili) Tipiki Baha (S) Synag esasynda
    Goss (45°) 43 43 ASTM D2457
    Duman 16% 16% ASTM D1003

    Hukuk beýannamasy

    Tis(nonilfenolfosfit (TNPP)CAS#26523-78-4 bu önümde EoonMobil tarapyndan bilgeşleýin ulanylmaýar. Bu önümiň barlygy yzygiderli barlanmasa-da, önümiň düzümi baradaky bilime esaslanyp, bu maddanyň bolmagyna garaşylmaýar. Şeýle-de bolsa, bu maddanyň ExxonMobl tarapyndan bu önümde halkara derejesinde ulanylmaýandygy, çig malyň we/ýa-da önümçilik prosesiniň aýratyn aýratynlyklary netijesinde bu maddanyň az derejesiniň bolmagynyň mümkindigini aradan aýyrmaýar.
    Bu önüm lukmançylyk maksatly ulanylyşlarda ulanmak üçin niýetlenmedik we şeýle ulanylyşlarda ulanylmaly däldir.
    Azyk bilen aragatnaşyk üçin arzalaryň laýyklygy barada ExxonMobil Chemical müşderi hyzmaty wekiliňiz bilen habarlaşyň (meselem, FDA, ÝB, HPFB)

    Gaýtadan işlenýän beýannama

    Flm (1 mil/254 mikron) 2.5:1 üfleme gatnaşygy bolan, ereme temperaturasy 403°F (206℃) bolan 2.5 dýuým (63.5 mm) üflenen plýonka çyzygynda ýasaldy, 60 mil (1.52 mm) galyp aralygy 10 funt/sag/n galyp aýlanyş tizliginde (1.79 kg/sag/sm).

    Bellikler

    Tipiki häsiýetler: bulary tehniki şertler hökmünde kabul etmeli däldir.